RE: Salvaging -purifying mixed alloys ?
Lead molecules will only adhere so much tin, or other metals. There are ways to refine it by making slurs like refining gold or other precious metals something you can't do in a lead pot by just fluxing or skimming. You can get some of the excess out but far from all of it.
The reason a dog has so many friends is because he wags his tail instead of his tongue.
Reply


Messages In This Thread
Salvaging -purifying mixed alloys ? - by J.B. - 09-01-2013, 10:00 PM
RE: Salvaging -purifying mixed alloys ? - by J.B. - 09-01-2013, 10:57 PM
RE: Salvaging -purifying mixed alloys ? - by Kurt - 09-02-2013, 10:45 AM
RE: Salvaging -purifying mixed alloys ? - by Kurt - 09-02-2013, 06:28 PM
RE: Salvaging -purifying mixed alloys ? - by john olsen - 11-08-2013, 01:24 AM
RE: Salvaging -purifying mixed alloys ? - by john olsen - 11-08-2013, 01:28 AM
RE: Salvaging -purifying mixed alloys ? - by Kurt - 11-08-2013, 10:31 AM
RE: Salvaging -purifying mixed alloys ? - by Shadow 4 - 11-11-2013, 12:54 AM